请问TPV的注塑工艺

2024-12-16 17:47:15
推荐回答(2个)
回答1:

使用前烘干80-100摄氏度3小时。加工温度200度上下,可适当调节10-15摄氏度。

回答2:

injection pressure and holding should be low. Otherwise it will cause flash on the part.
normally you should use low mold temperature less than 30 degree.